Materiaal Dimensie (mm) Lengte (mm) Cijfer
L 25 x 25 x 4 12000 S235JR/S275JR
L 30 x 30 x 3 12000 S355
L 30 x 30 x 4 12000 S235JR/S275JR
L 30 x 30 x 4 12000 S355
L 35 x 35 x 4 12000 S355
L 35 x 35 x 5 12000 S355
L 40 x 40 x 4 12000 S235JR/S275JR
L 40 x 40 x 4 12000 S355
L 40 x 40 x 5 12000 S235JR/S275JR
L 40 x 40 x 5 12000 S355
L 50 x 50 x 5 12000 S355
L 50 x 50 x 6 12000 S235JR/S275JR
L 50 x 50 x 6 12000 S355
L 60 x 60 x 10 12000 S355
L 60 x 60 x 5 12000 S355
L 60 x 60 x 6 12000 S355
L 60 x 60 x 8 12000 S235JR/S275JR
L 60 x 60 x 8 12000 S355
L 65 x 65 x 5 12000 S355
L 65 x 65 x 6 12000 S355
L 65 x 65 x 7 12000 S355
L 65 x 65 x 8 12000 S355
L 70 x 70 x 10 12000 S355
L 70 x 70 x 6 12000 S355
L 70 x 70 x 7 12000 S355
L 70 x 70 x 8 12000 S235JR/S275JR
L 70 x 70 x 9 12000 S235JR/S275JR
L 75 x 50 x 5 12000 S355
L 75 x 50 x 6 12000 S355
L 75 x 50 x 7 12000 S235JR/S275JR
L 75 x 50 x 7 12000 S355
L 75 x 50 x 8 12000 S355
L 75 x 50 x 9 12000 S355
L 75 x 75 x 10 12000 S355
L 75 x 75 x 6 12000 S235JR/S275JR
L 75 x 75 x 6 12000 S355
L 75 x 75 x 7 12000 S355
L 75 x 75 x 8 12000 S355
L 80 x 40 x 6 12000 S355
L 80 x 80 x 10 12000 S235JR/S275JR
L 80 x 80 x 10 12000 S355
L 80 x 80 x 6 12000 S355
L 80 x 80 x 8 12000 S355
L 90 x 60 x 6 12000 S355
L 90 x 60 x 8 12000 S235JR/S275JR
L 90 x 90 x 10 12000 S355
L 90 x 90 x 11 12000 S355
L 90 x 90 x 12 12000 S355
L 90 x 90 x 13 12000 S355
L 90 x 90 x 8 12000 S355
L 90 x 90 x 9 12000 S355
L 100 x 100 x 10 12000 S355
L 100 x 100 x 11 12000 S355
L 100 x 100 x 12 12000 S355
L 100 x 100 x 16 12000 S355
L 100 x 100 x 8 12000 S355
L 100 x 50 x 10 12000 S235JR/S275JR
L 100 x 50 x 10 12000 S355
L 100 x 50 x 6 12000 S235JR/S275JR
L 100 x 50 x 6 12000 S355
L 100 x 50 x 8 12000 S355
L 100 x 65 x 10 12000 S355
L 100 x 65 x 7 12000 S355
L 100 x 65 x 8 12000 S355
L 100 x 65 x 9 12000 S355
L 100 x 75 x 10 12000 S355
L 100 x 75 x 11 12000 S355
L 100 x 75 x 12 12000 S355
L 100 x 75 x 7 12000 S235JR/S275JR
L 100 x 75 x 7 12000 S355
L 100 x 75 x 8 12000 S355
L 100 x 75 x 9 12000 S355
L 110 x 110 x 10 12000 S355
L 110 x 110 x 12 12000 S355
L 120 x 120 x 10 12000 S355
L 120 x 120 x 12 12000 S235JR/S275JR
L 120 x 120 x 12 12000 S355
L 120 x 120 x 15 12000 S235JR/S275JR
L 120 x 120 x 15 12000 S355
L 120 x 120 x 8 12000 S355
L 120 x 80 x 10 12000 S355
L 120 x 80 x 12 12000 S355
L 120 x 80 x 8 12000 S235JR/S275JR
L 120 x 80 x 8 12000 S355
L 125 x 75 x 10 12000 S355
L 125 x 75 x 12 12000 S355
L 125 x 75 x 8 12000 S355
L 130 x 130 x 10 12000 S355
L 130 x 130 x 12 12000 S355
L 130 x 130 x 14 12000 S235JR/S275JR
L 140 x 140 x 13 12000 S355
L 150 x 100 x 10 12000 S355
L 150 x 100 x 12 12000 S355
L 150 x 100 x 14 12000 S355
L 150 x 100 x 15 12000 S355
L 150 x 150 x 10 12000 S235JR/S275JR
L 150 x 150 x 10 12000 S355
L 150 x 150 x 14 12000 S235JR/S275JR
L 150 x 150 x 14 12000 S355
L 150 x 150 x 15 12000 S355
L 150 x 150 x 16 12000 S235JR/S275JR
L 150 x 150 x 16 12000 S355
L 150 x 150 x 18 12000 S355
L 150 x 150 x 20 12000 S235JR/S275JR
L 150 x 150 x 20 12000 S355
L 150 x 75 x 10 12000 S355
L 150 x 75 x 11 12000 S355
L 150 x 75 x 12 12000 S355
L 150 x 75 x 15 12000 S235JR/S275JR
L 150 x 75 x 15 12000 S355
L 150 x 75 x 9 12000 S355
L 150 x 90 x 10 12000 S355
L 150 x 90 x 12 12000 S355
L 150 x 90 x 15 12000 S235JR/S275JR
L 150 x 90 x 15 12000 S355
L 160 x 160 x 15 12000 S235JR/S275JR
L 160 x 160 x 15 12000 S355
L 160 x 160 x 17 12000 S235JR/S275JR
L 160 x 160 x 17 12000 S355
L 160 x 80 x 10 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S235JR/S275JR
L 180 x 180 x 16 12000 S355
L 180 x 180 x 18 12000 S235JR/S275JR
L 180 x 180 x 18 12000 S355
L 180 x 180 x 20 12000 S235JR/S275JR
L 180 x 180 x 20 12000 S355
L 180 x 180 x 22 12000 S355
L 180 x 90 x 10 12000 S355
L 200 x 100 x 10 12000 S235JR/S275JR
L 200 x 100 x 10 12000 S355
L 200 x 100 x 12 12000 S235JR/S275JR
L 200 x 100 x 12 12000 S355
L 200 x 100 x 14 12000 S235JR/S275JR
L 200 x 100 x 14 12000 S355
L 200 x 100 x 15 12000 S235JR/S275JR
L 200 x 100 x 15 12000 S355
L 200 x 100 x 16 12000 S235JR/S275JR
L 200 x 100 x 16 12000 S355
L 200 x 150 x 12 12000 S235JR/S275JR
L 200 x 150 x 12 12000 S355
L 200 x 150 x 15 12000 S235JR/S275JR
L 200 x 150 x 15 12000 S355
L 200 x 200 x 16 12000 S235JR/S275JR
L 200 x 200 x 16 12000 S355
L 200 x 200 x 18 12000 S235JR/S275JR
L 200 x 200 x 18 12000 S355
L 200 x 200 x 20 12000 S235JR/S275JR
L 200 x 200 x 20 12000 S355
L 200 x 200 x 22 12000 S235JR/S275JR
L 200 x 200 x 22 12000 S355
L 200 x 200 x 24 12000 S235JR/S275JR
L 200 x 200 x 24 12000 S355
L 200 x 200 x 26 12000 S235JR/S275JR
L 200 x 200 x 26 12000 S355
L 200 x 200 x 28 12000 S235JR/S275JR
L 200 x 200 x 28 12000 S355
L 200 x 200 x 34 12000 S355
L 250 x 250 x 18 12000 S235JR/S275JR
L 250 x 250 x 18 12000 S355
L 250 x 250 x 20 12000 S235JR/S275JR
L 250 x 250 x 20 12000 S355
L 250 x 250 x 22 12000 S235JR/S275JR
L 250 x 250 x 22 12000 S355
L 250 x 250 x 24 12000 S235JR/S275JR
L 250 x 250 x 24 12000 S355
L 250 x 250 x 25 12000 S355
L 250 x 250 x 26 12000 S235JR/S275JR
L 250 x 250 x 26 12000 S355
L 250 x 250 x 28 12000 S355
L 250 x 250 x 30 12000 S355
L 250 x 250 x 35 12000 S355
L 250 x 90 x 10 12000 S235JR/S275JR
L 250 x 90 x 10 12000 S355
L 250 x 90 x 12 12000 S235JR/S275JR
L 250 x 90 x 12 12000 S355
L 250 x 90 x 14 12000 S235JR/S275JR
L 250 x 90 x 14 12000 S355
L 250 x 90 x 16 12000 S235JR/S275JR
L 250 x 90 x 16 12000 S355
PR HEA 100 12000 S235JR/S275JR
PR HEA 100 12000 S355
PR HEA 120 12000 S235JR/S275JR
PR HEA 120 12000 S355
PR HEA 140 12000 S235JR/S275JR
PR HEA 140 12000 S355
PR HEA 160 12000 S235JR/S275JR
PR HEA 160 12000 S355
PR HEA 180 12000 S235JR/S275JR
PR HEA 180 12000 S355
PR HEA 200 12000 S235JR/S275JR
PR HEA 200 12000 S355
PR HEA 220 12000 S355
PR HEA 260 12000 S355
PR HEA 300 12000 S355
PR Heb 100 12000 S235JR/S275JR
PR Heb 100 12000 S355
PR Heb 120 12000 S235JR/S275JR
PR Heb 120 12000 S355
PR HEB 140 12000 S235JR/S275JR
PR HEB 140 12000 S355
PR Heb 160 12000 S235JR/S275JR
PR Heb 160 12000 S355
PR Heb 180 12000 S235JR/S275JR
PR HEB 200 12000 S235JR/S275JR
PR HEB 200 12000 S355
PR IPE 100 12000 S235JR/S275JR
PR IPE 120 12000 S235JR/S275JR
PR IPE 140 12000 S235JR/S275JR
PR IPE 160 12000 S235JR/S275JR
PR IPE 160 12000 S235JR/S275JR
PR IPE 220 12000 S355
PR IPE 240 12000 S355
PR IPE 270 12000 S355
PR IPE 300 12000 S355
PR IPE 550 12000 S355
PR IPE 80 12000 S235JR/S275JR
PR IPN 360 12000 S235JR/S275JR
PR IPN 80 12000 S235JR/S275JR
PR UPE 80 12000 S355
PR UPE 100 12000 S355
PR UPE 120 12000 S355
PR UPE 140 12000 S355
PR UPE 160 12000 S355
PR UPE 180 12000 S355
PR UPE 200 12000 S235JR/S275JR
PR UPE 200 12000 S355
PR UPE 220 12000 S355
PR UPE 240 12000 S355
PR UPE 300 12000 S355
PR UPE 400 12000 S355

We hebben meer dan 10000 m² opslagruimte en onderhouden nauwe relaties met honderden leveranciers en staalfabrieken in heel Europa en wereldwijd. Dit stelt ons in staat om snel elke omvang of cijfer te leveren die niet beschikbaar is in onze aandelen tegen de beste prijzen en doorlooptijden.

Onze voorraad omvat voornamelijk:

• Structurele staalproducten (IPE, UPE, UPN, HEA, HEB, Gelijke en ongelijke invalshoeken) in de klassen S235JR, S275JR, S355J2

• Hot-gerolde stalen vellen en spoelen (3 mm tot 12 mm, DD11/S235JR+N/S355MC, ingelegd en geolied)

• Gegalvaniseerde staalbladen en spoelen (0. 5mm tot 4mm, dx 51+ z)

• Koud gerolde staalbladen en spoelen (DC01)

• T-bars, platte staven, ronde staven, vierkante staven en holle secties (EN 10219 of EN 10210)

• Roestvrijstalen producten (bars, vellen, platen)

• Zware platen (6 mm tot 300 mm in elke maat en graad)