S690QL steel is a high strength, low alloy structural steel that has been designed for use in heavy-duty applications such as cranes, bridges, and other structures. This steel grade is also known as Quenched and Tempered Steel, which refers to its heat treatment process.

 

S690QL steel is a high yield strength steel with a minimum yield strength of 690 MPa. It has excellent weldability, formability, and toughness, which makes it suitable for use in a variety of heavy-duty applications. This steel grade is also known for its high resistance to fatigue and abrasion.

 

 

 

 

  • Chemical Composition – EN10025 S690QL
C P S B N V
0.20 0.80 1.70 0.020 0.010 0.005 1.50 0.50 0.70 0.015 0.06 2.0 0.05 0.12 0.15

 

  • Mechanical Properties – EN10025 S690QL
Elongation A5 % minimum
3mm to 50mm 690 770 – 940 14 30 @ -40º C
50mm to 100mm 650 760 – 930 14 30 @ -40º C
100mm to 150mm 630 710 – 900 14 30 @ -40º C

 

 

Equivalent grades of steel S690QL (1.8928)

 

 



-





S690QL
A709-100
TStE690V
E690T
E690TFP
S690T
FeE690VKT
2625
E690

 

 

Benefits of S690QL steel plate

 

 

S690QL ultra high strength steel : S690QL steel has a high yield strength of 690 MPa, which makes it suitable for use in heavy-duty applications that require high strength and durability.

 

: S690QL steel has excellent weldability, which makes it easy to fabricate and assemble.

 

S690QL steel has good toughness, which provides resistance to impact and fatigue, making it suitable for use in heavy-duty applications.

 

S690QL steel has good corrosion resistance, which makes it suitable for use in offshore structures and other applications where exposure to harsh environments is expected.

 

 

Applications of S690QL Ultra High Strength Steel

 

 

S690QL ultra high strength steel

In the construction industry, S690QL is used for building structures that require high load-bearing capacity and resilience, such as bridges, high-rise buildings, and stadiums. Its ability to withstand heavy loads without compromising structural integrity makes it an invaluable material for infrastructure projects.

 

The manufacturing of heavy machinery, including cranes, earth-moving equipment, and mining machinery, benefits from the high strength and durability of S690QL. It ensures that these machines can operate under extreme conditions and carry heavy loads efficiently.

 

S690QL ultra high strength steel

In the transportation sector, S690QL is used to produce components for heavy-duty trucks, trailers, and other vehicles that require enhanced strength and durability. Its use leads to safer, more reliable vehicles capable of handling demanding tasks.

 

S690QL ultra high strength steel stands out as a material of choice for numerous high-performance applications due to its exceptional strength, toughness, weldability, and resistance to wear and tear. Its advantages extend beyond just performance, offering cost savings and extended service life, making it an excellent investment for any project requiring superior material properties. Whether in construction, heavy machinery, or transportation, S690QL provides the reliability and efficiency needed to meet today's engineering challenges.

 

 

alloy@gneesteelgroup.com. We are more than happy to assist you.

 

What is the difference between S690Q and S690QL?

S690Q: Minimum impact toughness tested at -20℃ (30J average). → Typical Use: Cranes in temperate climates, quarry equipment. S690QL: Certified for -40℃ and below (>=40J impact toughness). → Critical Use: Arctic pipelines, offshore platforms, mining vehicles in Siberia.

What grade is S690QL material?

S690QL is a high strength quenched and tempered steel grade that complies to steel specification EN 10025. The designation S690QL refers to a minimum yield strength of 690 MPa.

What is S690 grade steel?

S690 high yield & fine grain steel plate is a high strength, quenched and tempered fine-grain structural steel. Structural steel S690 is used in structures that must withstand very heavy loads. This grade is meant for structures where weight savings is important.

What is the equivalent of S690 steel?


ASTM A514, EN 10149-2 Grade S700MC, AS/NZS 3579 Grade 700, AM 700, Bisalloy 80.

What is the price of S690QL material?

S690QL High Strength Steel Plates, Thickness: 5mm to 150mm at 5,600-13,500 CNY per tonne (approx. 5.6-13.5 CNY per kilogram)/440-900 USD per tonne (approx. 0.44-0.90 USD per kilogram)

What is the hardness of S690 QL steel?

S690QL steel stockholders and suppliers. S690QL is a quenched and tempered high strength steel supplied in full plates or cut pieces with delivery to the whole of the UK. With its high yield of minimum 690MPa it offers better strength than standard carbon steel grades.

What is the effective use of high strength S690 steel in construction?

The high strength S690 steels have an excellent strength-to-self-weight ratio, and they are highly efficient to be used in heavily loaded structures. Typical applications include piles and columns in buildings and supporting members in bridges.

What is the difference between S890QL and S690QL?

S690QL, S890QL, and S960QL are all water quenched and tempered steels that comply with the EN10025:6:2004 specification. These ultra high strength steels have a minimum yield strength of 690 MPa, 890 MPa, and 960 Mpa respectively, making them ideal for use in the haulage sector.

What is the difference between S700MC and S690ql?

The S700MC Steel is basically a structural steel plate developed especially for applications requiring high yield strength. They are used for several load bearing applications. The S690ql is a low alloy structural steel which is high in strength and comes with good weldability.

What is the yield strength of s690 steel?

690 MPa.

Yield strength of 690 MPa. Used in structures bearing extremely heavy loads, such as bridges, offshore drilling rigs and buildings, as well as in heavy construction equipment and cranes.

 

P265GH+410,S355JR+410,A516Gr70+316,
A537CL1+304L,Q235B+304L,Q345B+304,
A516Gr70(NACE)+410,A537CL1+904L,
A537CL1+316L,A516Gr70+304L,A537CL1+304
,A516Gr70+410,A516Gr70+904L
2-300mm(Based plate),1-50mm(Composited plate) / UT, AR, TMCP.Normalized, Quenched and Tempered,Z Direction Test, Charpy V-Notch impact TestThe Third Party Test , Coated or Shot Blasting and Painting.
Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo 6 - 350 5788.56 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
High-Strength Plate WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E 8 - 120 3086.352
Wear-Resistant Plate NM360, NM400, NM450, NM500 6 - 150 3866.297
Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 8 - 200 2853.621 Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness