  S890Q, S890QL, and S890QL1 are high-strength structural steels (EN 10025-6 standard) with a minimum yield strength of 890 MPa, differentiated by their required impact toughness at progressively lower temperatures: S890Q (basic -20℃), S890QL (better -40℃), and S890QL1 (superior -60℃), making them suitable for increasingly colder climates, all achieved through quenching and tempering (Q).

 

  • 890 MPa

.

 

 

1. S890Q Steel Plate

–20℃

Standard high-strength structural applications

Cost-effective, widely used, good balance of strength and toughness

S890Q is suitable for heavy machinery, cranes, and structures operating in normal or moderately cold environments.

S890QL Steel Plate

2. S890QL Steel Plate

–40℃

Structures in colder climates or higher safety-demand projects

Improved low-temperature toughness and crack resistance

S890QL provides a higher safety margin than S890Q, making it ideal for offshore platforms, wind energy structures, and cold-region construction.

3. S890QL1 Steel Plate

–60℃

S890QL1 is used in Arctic, sub-zero, or highly demanding environments where structural integrity at very low temperatures is critical.

 

Toughness: The Key Differentiator (Q vs QL vs QL1)

 

low-temperature toughness-a critical factor for applications in cold climates or harsh environments.

 

The suffixes "Q", "QL", and "QL1" denote increasing toughness requirements, measured by Charpy V-notch impact tests:

S890Q

-20℃

40 J

Mild-temperature environments: construction machinery, bridge components, and general heavy engineering.

S890QL

-40℃

60 J

Cold regions: offshore structures, winter-resistant construction equipment, and mid-latitude wind turbines.

S890QL1

-60℃

60 J

Extreme cold: Arctic/offshore oil platforms, high-altitude wind farms, and polar-region mining equipment.

 

GNEE Steel's S890QL and S890QL1 use refined steelmaking processes (e.g., ladle refining, vacuum degassing) to reduce impurities, enhancing toughness without compromising strength. This makes our plates ideal for projects in harsh, low-temperature conditions.

 

Equivalent Grades: Global Standards Cross-Reference

 

For international projects, understanding equivalent grades is essential. Below is a quick reference for S890Q, S890QL, and S890QL1 across major standards-verified by GNEE Steel's technical team:

 

: All three grades are equivalent to A514 Grade Q (quenched & tempered, >=890 MPa yield strength).

: Corresponding to SSAB Domex 100Q/QL/QL1 or JFE-HITEN 1000Q/QL.

: S890Q ≈ Q960C; S890QL ≈ Q960D; S890QL1 ≈ Q960E (per GB/T 16270).

: Directly covered by EN 10025-6, with QL/QL1 as upgraded toughness variants of Q.

 

 

  • S890Q for standard high-strength structural applications
  • S890QL
  • S890QL1 for extreme low-temperature environments

If unsure, consulting a professional supplier can help avoid over-specification or underperformance.

 

 

 

S890Q, S890QL, or S890QL1 high-strength structural steel plates, GNEE Steel is your reliable partner. Contact us today for expert advice, fast quotations, and dependable global delivery.

 

GNEE Steel – High Strength Solutions You Can Trust.

 

 

Carbon and Low-alloy High-strength Steel1

 

 

PackingShipping

PackingShipping1

 

 

GNEE Global Exhibition Record

 

 

 
 

 

GNEE Steel also supplies a variety of high-strength steel plates, such as A514 Grade F, A572 Grade 50, A588 Grade A, S355JR, S690Q, SS400, S690QL, Q345B, Q345E, etc. If you want to know more about other types of steel plates, you can call the consultation hotline at +8615824687445 or send an email to alloy@gneesteelgroup.com. You are welcome to consult us, and we are very willing to answer your questions.