A Guide of EN 10025-6 S890QL Structural Steel Plate

Dec 31, 2025 Laat een bericht achter

  ↵S890QL Steel Plates are manufactured in compliance with EN 10025:6:2004 standard ensuring a high yield steel. S890QL Plate is heat treated using quenching and tempering techniques and displays good welding and bending properties.

 

This type of steel, which is well over three times the strength of a basic S275 structural steel, is still relatively easy to weld and fabricate.

  • EN 10025 includes a range of high strength quenched and tempered steel grades.
  • Minimum yield strength of 890 MPa.

 

GNEE Steel and S890QL Steel Plate
GNEE Steel holds a substantial stock of S890QL steel plates in the China. These plates are frequently sold as cut to size pieces and shapes which are produced on the company's computer controlled cutting machines but plates straight from stock for fabrication by our customers are also readily available.

 

Advantages of Using S890QL Steel Plate

Choosing EN 10025-6 S890QL offers several project-level benefits:

.

S890QL Steel Plate

 

EN10025-6 S890QL quenched and tempered steel plate Chemical composition

C % P % S % N % B %
S890QL 0.200 0.800 1.700 0.020 0.010 0.015 0.005 1.500
V %    
0.500 0.700 0.060 2.000 0.050 0.120 0.150    


EN10025-6 S890QL quenched and tempered steel plate mechanical properties

 
S890QL 8mm-50mm Min 890Mpa 940-1100Mpa 11% -40 Min 30J
  51mm-100mm Min 830Mpa 880-1100Mpa 11% -40 Min 30J
  101mm-150mm Min 800Mpa 820-1000Mpa 11% -40 Min 30J

 

S890QL High Steel Structures Plate of Specification :

: The standard governing S890QL steel is often EN 10026-6.

: S890QL (also known as S890Q).

Available in various thicknesses, typically ranging from 1 mm to 50 mm.

: Commonly available widths are from 1500 mm to 5000 mm.

: Lengths usually range from 1200 mm to 12000 mm.

: Quenched and Tempered (Q+T).

 

 

We find that the category of steel plate that EN 10025 S890QL falls into is called different things by different engineers. Plate of this type is variously described as:
• S890QL High Strength Quenched and Tempered Steel Plate
• S890QL High Yield Quenched and Tempered Steel Plate
• S890QL High Strength Structural Steel Plate,
• S890QL High Yield Structural Steel Plate
• S890QL High Strength Low Alloy Steel Plate
• S890QL HSLA

 

Typical Applications of S890QL Structural Steel Plate

 

Thanks to its high performance and reliability, EN 10025-6 S890QL is widely used in:

  • Lifting booms and load-bearing arms
  • High-stress bridges and industrial structures

 

, S890QL is often preferred over S890Q due to its superior low-temperature toughness.

 

 

EN 10025-6 S890QL structural steel plate is an advanced high-strength material designed for the most demanding structural applications. With its outstanding yield strength, excellent low-temperature toughness, and proven reliability, it is an ideal choice for modern heavy engineering projects.

 

reliable S890QL steel plate supplier today for expert consultation, competitive quotations, and dependable global delivery.

 

GNEE Steel – Powering Structures with High Strength and Trust.

 

 

Q1: What is S890Q steel plate?

A:S890Q is a high-strength structural steel plate according to EN 10025-6, supplied in quenched and tempered (Q) condition, with a minimum yield strength of 890 MPa.

Q2: What is the material number of S890Q?

A:The European material number for S890Q is 1.8940.

Q3: Is S890Q considered non-alloy steel?

A:Yes. Under EN classification, S890Q is listed as non-alloy structural steel, although small alloying elements are added for strength and toughness control.

Q4: What thickness range is available for S890Q steel plate?

A:Common supply thickness ranges from 6 mm to 150 mm, depending on mill capability and standard requirements.

 

 

Carbon and Low-alloy High-strength Steel1

 

 

PackingShipping

PackingShipping1

 

 

GNEE Global Exhibition Record

 

 

 
 

 

GNEE Steel also supplies a variety of high-strength steel plates, such as A514 Grade F, A572 Grade 50, A588 Grade A, S355JR, S690Q, SS400, S690QL, Q345B, Q345E, etc. If you want to know more about other types of steel plates, you can call the consultation hotline at +8615824687445 or send an email to alloy@gneesteelgroup.com. You are welcome to consult us, and we are very willing to answer your questions. 

 

 

S890QL high tensile steel, Structural S890QL plates, S890QL steel sheets, S890QL steel fabrication, S890QL plate suppliers, S890QL steel applications, S890QL welding techniques, S890QL steel properties, S890QL heat treatment, S890QL steel standards, S890QL structural uses, S890QL chemical composition, S890QL mechanical properties, S890QL thickness options, S890QL steel bending, S890QL machining services, S890QL cutting methods, S890QL high strength steel, S890QL steel pricing, S890QL plate inventory, S890QL industrial uses, S890QL engineering uses, S890QL construction materials, S890QL manufacturing process, S890QL steel performance

 

S890QL High Steel Structures Plate We Supply Globally:

S890QL High Steel Structures Plate to various cities like Faridabad, Jaipur, Chandigarh, Hyderabad, Navi Mumbai, Jamshedpur, Indore, Ludhiana, Abu Dhabi, Noida, Visakhapatnam, Kanpur, New Delhi, Pune, Bengaluru, Howrah, Surat, Kolkata, Thiruvananthapuram, Gurgaon, Ranchi, Baroda, Chennai, Ahmedabad, Haryana, Nagpur, All Over India.